Evaluation of the effect of metal primers and type of resin cement on the bond strength to zirconia
Abstract
This study evaluated the influence of a metal primer application and the type of resin cement on the bond strength (BS) to yttrium-stabilized tetragonal zirconia, after 24 hours and 6 months of water storage. Zirconia plates (13mmX5mmX1mm) were used in 8 experimental groups (n=10). The micro-shear bond strength test was used in this study. The results were analyzed by three-way Anova (primer application, type of resin cement, storage time) and Tukey test (?=0.05). The primer application did not influence the BS and the resin cement Clearfil SA Cement resulted in higher BS to zirconia. The storage in water for 6 months reduced the BS for all groups.
Keywords
Zircônia, Resistência de união, Cimento resinoso
Full Text:
PDF (Português (Brasil))DOI: http://dx.doi.org/10.18363/rbo.v69n1.p.15
Copyright (c) 2016 Revistas
e-ISSN: 1984-3747
The Brazilian Journal of Dentistry is licensed with a Creative Commons Atribuição-NãoComercial 4.0 Internacional